Kafin rufe murfin ƙarshen waje najanareta, pre-cika sawun HDJ892 sutturar sawun HDJ892 a cikin secking na seforing na hadin gwiwa na haɗin gwiwa, sa'an nan kuma ƙara ɗaure raga a ko'ina. To sai a yi amfani da kayan aiki na musamman don yin amfani da HDJ892 Sealant a cikin sealing tsintsiya (Hanyar Idra Idga don fara sannu a hankali, sannan kuma ya kwarara daga rami mai kyau.
Siginan na kwararru na jan Gendren
Bayyanar: launin toka-baki jiki, babu ƙazanta
Haskaka mai zafi: 80 ℃ ba ya bakin ciki, baya gudana
Filin filastik: 6 ± 2 sec
Bala'i na hatimi:> 0.6mpsa
1. Ya kamata a sanya hdj892 Sannu a cikin tsabta, busasshiyar, mai bushe, da kuma kariya daga rana, ruwan sama, zafi da matsin lamba.
2. Lokacin da HDJ892selantAn adana a cikin akwati na asali da aka rufe, daga ranar isarwa, lokacin ajiya shine: watanni 18 a dakin da zazzabi (18 ~ 32 ℃); Watanni 24 a ƙarancin zafin jiki (2 ~ 10 ℃).
3. Kare Hydrogen Hydrogen ya rufe slot Sealant Hdj892 ya kamata a ɗora shi a cikin motar da aka rufe, kuma kada a kiyaye shi da matsi.
Kunshin na jan janareta hydrogen hating slot sealant hdj892:
1. Rike kowane 1kg na sealant tare da fim 0.2mm polyethylene tare da sanya shi cikin akwatin alkawarin polyethylene mai rufe filastik. Sanya akwatin polyethylene a cikin akwatin filastik a cikin katun ko katako na katako bisa ga adadin da mai amfani da mai amfani yake buƙata.
2. Ya kamata a yiwa alama alama: Sunan mai samarwa, samfurin samfuri da suna, da kuma nauyin da ake ciki, da sauransu. Jira.
Lokacin ajiya a zazzabi dakin (2 ~ 10 ℃): watanni 24